About the Case

Patient requests a nonmetallic alternative for full coverage crown on tooth #18. As a class 4 material, 3M™ Chairside Zirconia exhibits a flexural strength of >800 MPa with a fracture toughness of KI>3.5.

Preparation with margination

Preparation with margination.

Proprosal with occlusion

Proprosal with occlusion.

Proposal with sprue

Proposal with sprue.

Milling timeframe

Milling timeframe.

CEREC SpeedFire oven - occlusal down

CEREC® SpeedFire oven – occlusal down.

Polished with DiaShine

Polished with DiaShine.

Sintered polished - note lower value

Sintered polished – note lower value.

Post cementation cleanup

Post cementation cleanup.

You May Also Like

Clinical Case: Ensuring Efficiency and High-quality Results with Proactive Curing Light Testing

Using 3M™ Elipar™ DeepCure-S LED Curing Light.

Clinical Case: Treatment of a Non-carious Cervical Lesion with Glass Ionomer Restorative

Using 3M™ Ketac™ Universal Aplicap™ Glass Ionomer Restorative.

Clinical Case: Selective-etch Adhesive Cementation of Chairside CAD/CAM Glass Ceramic Inlays

Using 3M™ RelyX™ Universal Resin Cement and 3M™ Scotchbond™ Universal Plus Adhesive using the selective-etch technique.